PEG pretreated Ti3C2 MXene

source:beike new material Views:3529time:2020-08-10 QQ Academic Group: 1092348845

The concentration of MXene colloid was determined by weighing specific amounts of dispersion though freezedrying at −60 °C for 48 h. For preparing PEG pretreated Ti3C2 MXene,the given mass of PEG solution (PEG/MXene = 1/2, w/w) was poured into MXene colloid with magnetic stirring for 60 min and then freezedried at −60 °C for 96 h.


 

Reminder: Beijing Beike New Material Technology Co., Ltd. supplies products only for scientific research, not for humans
All rights reserved © 2019 beijing beike new material Technology Co., Ltd 京ICP备16054715-2号
advisory
phone
Email:mxenes@163.com
Tel:+86-17715390137
scan

scan
WeChat