Spatiotemporally Engineered Microneedles Promote Mucosal Regeneration after Tracheal Mucosal Injury via Microenvironment Remodeling

source:material synthesis Views:206time:2026-11-09material synthesis: 1092348845

已传文件:photo/1794201718.png

This study was published in Bioactive Materials under the title “Spatiotemporally engineered microneedle for microenvironment remodeling propels mucosal regeneration after tracheal mucosal injury”.



Remodeling the mucosal microenvironment is a critical step in severe tracheal mucosal injury (TMI), which can trigger a cascade of pathological events including infection, inflammation, oxidative stress and microvascular disruption. Current therapeutic strategies for TMI mainly focus on anti‑infection or anti‑inflammatory pathways, or rely on surgical intervention to manage complications such as stenosis. Nevertheless, precise regulation of the mucosal microenvironment remains insufficient, and the unique anatomical structure of the trachea hinders drug delivery and the maintenance of therapeutic concentrations. To address these challenges, a spatiotemporally engineered bilayer microneedle (MN) based on gelatin (Gel) functionalized with silver nicotinate (AgNA) and magnesium gallate (MgGA) metal–organic frameworks (MOFs) was developed. Temporally, the Gel‑AgNA/MgGA MN sustains therapeutic activity through sequential degradation of gelatin and MOFs. Spatially, the layered loading of AgNA and MgGA MOFs enables targeted modulation of the mucosal microenvironment. In addition, the Gel‑AgNA/MgGA MN can efficiently penetrate the mucosa and firmly adhere to the tissue surface. In vitro experiments demonstrate that AgNA MOFs at the microneedle base eradicate bacteria; MgGA MOFs at the microneedle tip reduce reactive oxygen species (ROS) accumulation, promote M2 macrophage polarization, and upregulate the expression of pro‑angiogenic genes. In vivo, the Gel‑AgNA/MgGA MN improves the survival rate of rabbits, restores respiratory function, and facilitates epithelial and microvascular regeneration. This study provides insights into mucosal microenvironment remodeling and offers a potential therapeutic strategy for TMI.


Literature Spotlight

Figure 1

Schematic illustration of the spatiotemporally engineered gelatin‑silver nicotinate/magnesium gallate microneedle (Gel‑AgNA/MgGA MN), which remodels the mucosal microenvironment after tracheal mucosal injury in rabbits by alleviating infection, inflammation and oxidative stress and promoting angiogenesis. Tracheal mucosal injury (TMI) triggers a cascade of pathological events, including infection, inflammation, oxidative stress and microvascular disruption, which collectively impair the microenvironment required for mucosal regeneration. Silver nicotinate (AgNA) exhibits potent antibacterial activity; magnesium gallate (MgGA), a chelate of magnesium ions and gallic acid, exerts synergistic anti‑inflammatory, antioxidant and pro‑angiogenic effects. To achieve spatiotemporal control of these therapeutic functions, a gelatin‑based bilayer microneedle (Gel‑AgNA/MgGA MN) is fabricated, in which AgNA is incorporated into the base and MgGA is embedded within the needle tips. When applied to rabbit tracheal mucosal injury, AgNA efficiently eliminates intraluminal bacterial colonization and inhibits biofilm formation. Meanwhile, MgGA that penetrates the submucosal tissue mitigates inflammation and oxidative stress and stimulates neovascularization. As the Gel‑AgNA/MgGA microneedle gradually degrades, therapeutic components are sustainably released to maintain its multifunctional effects. Collectively, this spatiotemporally engineered Gel‑AgNA/MgGA microneedle remodels the post‑injury tracheal microenvironment and facilitates mucosal regeneration.

Figure 2

Characterization of MgGA MOFs, AgNA MOFs and Gel‑AgNA/MgGA microneedles. (a) Representative SEM/EDS images of MgGA and AgNA MOFs. (b) X‑ray diffraction patterns of MgGA and AgNA MOFs. (c) Superoxide dismutase‑like (O₂∙⁻ scavenging) and catalase‑like (H₂O₂ scavenging) activities of MgGA MOFs. (d) SEM images of Gel and Gel‑AgNA/MgGA microneedles. (e) Fourier‑transform infrared (FTIR) spectra of Gel, Gel‑MgGA and Gel‑AgNA. (f) Hemolysis ratio of Gel, Gel‑AgNA, Gel‑MgGA and Gel‑AgNA/MgGA microneedles. (g) Fluorescence staining of Gel‑AgNA/MgGA microneedles with different heights. (h) Macroscopic and optical microscopic observation of microneedles. (i) Optical micrograph showing methylene‑blue‑stained microneedles penetrating tracheal mucosa. (j, k) Force‑distance curves of various microneedles. (l) Degradation rates of different microneedles.

Figure 3

Effects of gelatin‑AgNA/MgGA microneedles (Gel‑AgNA/MgGA MN) on oxidative stress, macrophage polarization and angiogenesis after treatment with gelatin (Gel), gelatin‑MgGA (Gel‑MgGA), or gelatin‑AgNA/MgGA microneedles (Gel‑AgNA/MgGA MN). (a) Representative fluorescence images of DCFH‑DA staining (reactive oxygen species (ROS) marker, green) in RAW264.7 cells and quantitative analysis of ROS levels (n = 3). (b–c) Immunofluorescence images and quantitative analysis of CD86⁺ and CD206⁺ macrophages in RAW264.7 cells after different treatments (n = 3). (d) Flow cytometry analysis of RAW264.7 macrophages (n = 3). (e) Schematic diagram of human umbilical vein endothelial cells (HUVECs) co‑cultured with various microneedles (MN). (f) Representative images and quantitative results of the Transwell assay in HUVECs (n = 3). (g) Representative images and quantitative results of the EdU assay in HUVECs (n = 3). (h) RT‑PCR analysis of angiogenesis‑related gene expression in HUVECs after 3 days of co‑culture with microneedles (n = 3).

Figure 4

Antibacterial activity of gelatin‑AgNA/MgGA microneedles (Gel‑AgNA/MgGA MN) against Escherichia coli and Staphylococcus aureus after treatment with Gel, Gel‑AgNA or Gel‑AgNA/MgGA MN. (a) Representative agar plate images and Syto9/PI staining results of bacteria after 24 h of treatment with different microneedles. (b, c) Colony counting and quantitative analysis of live/dead bacteria (n = 3). (d) Scanning electron microscopy (SEM) images of E. coli and S. aureus. (e) Protein leakage of bacteria under different treatments. (f) Crystal violet staining and live/dead staining of biofilms after various treatments. (g, h) Quantitative evaluation of biofilms, including absorbance at 570 nm and average thickness (n = 3). (i) Schematic illustration of the antibacterial mechanism of Gel‑AgNA/MgGA microneedles.



Reference Information

Bioactive Materials (IF 23.6)

Pub Date: 17 February 2026

DOI: 10.1016/j.bioactmat.2026.01.026


We specialize in custom fabrication of functional nanomedicinal materials. We conduct targeted development according to experimental requirements, with tunable material structure, particle size and surface modification. Full characterization services are available. Research proposals can be iteratively optimized with continuous technical support throughout the project. Our services support research programs including targeted delivery, bioimaging and nanotheranostics. Feel free to share your specifications for proposal evaluation.

Mr. Zhang: +86 17715390137

Mr. Chen: +86 18914047343



 

Reminder: Beijing Beike New Material Technology Co., Ltd. supplies products only for scientific research, not for humans
All rights reserved © 2019 beijing beike new material Technology Co., Ltd 京ICP备16054715-2号
advisory
phone
Email:mxenes@163.com
Tel:+86-17715390137
scan

scan
WeChat